Stateroom door varnishing - first diluted coat - 2011

 We turned over the door and scrapped off the varnish drools from varnishing the other side.
March 2011  - At Marina Cortez Harbor IslandSan Diego, CA

The sanded it and washed it again with TSP. The wiped it with 333 and then did the first coat diluted varnish coat. I may have diluted to much but no big deal. It was about 5:20 PM and outside so there was some light and no wind. 
 We will do another final coat to the gloss on the other side later. We wanted to keep moving on the varnishing so this side is needy in varnishing. No delays just keep up the coats.