First coats of Pettit Z Spar Flagship Varnish - 2015 Gloss on.
June 2019 -We are
currently in Paradise Village Marina in Banderas Bay Mexico (by Puerto Vallarta)
First coat of 50\50 that is why it is dull.
Second coat of 70\30 has a goiter look.
We had a thunder shower the night we put on the first coat. i do think it was protected enough with the first coat. Definitely do not want moisture under the varnish. I waited till the afternoon to put on the second coat and it was baking hot. It also would have backed out any moisture.
Mixed up 50\50 brew for the first coat.
And did I say it was HOT ans it is now summer!